Physical and strength properties of Fe/SiC composites under microwave hybrid sintering method
รหัสดีโอไอ
Creator Siti Nurul Adura DAUD
Title Physical and strength properties of Fe/SiC composites under microwave hybrid sintering method
Contributor Suraya Mohd TAHIR, Mohd Shamsul ANUAR, Che Nor Aiza JAAFAR, Mohd Zuhri Mohamed YUSOFF
Publisher Metallurgy and Materials Science Research Institute Chulalongkorn University
Publication Year 2562
Journal Title Journal of Metals Materials and Minerals
Journal Vol. 29
Journal No. 2
Page no. 70-78
Keyword Fe/SiC, Microwave hybrid sintering, Tensile strength, Shrinkage, Relative density
URL Website http://ojs.materialsconnex.com/index.php/jmmm/article/view/501
Website title Physical and strength properties of Fe/SiC composites under microwave hybrid sintering method | Daud | Journal of Metals Materials and Minerals
ISSN 8576149
Abstract Two different methods for the sintering of Fe/SiC composite prepared via uniaxial powder compaction are investigated in this work; the conventional furnace sintering and the microwave hybrid sintering methods. The important variables considered are the compositions of SiC in the Fe/SiC composite and the sintering temperatures used. The compositions of the SiC in the Fe/SiC used are 0, 10 and 20 wt. % and the sintering temperatures used are 1000?C, 1050?C, 1100?C and 1200?C. Damaged samples are obtained at the sintering temperatures of 1100?C and 1200?C for microwave hybrid method. For the undamaged samples obtained at 1000?C and 1050?C sintering temperatures, the physical and strength properties are studied. The physical properties of the sintered samples studied are the occurrence of shrinkage and swelling, the relative density and also their microstructure. The results show that the samples sintered under microwave hybrid process exhibit relatively higher shrinkage and swelling. The addition of SiC leads to the decrease in the relative densities of the sintered Fe/SiC samples. In addition, the tensile strengths of the Fe/SiC samples decrease with increasing SiC content. Microwave hybrid sintering produces relatively stronger samples by having relatively higher tensile strength values, especially for pure Fe and at 10 wt% SiC at 1050?C sintering temperature.
Metallurgy and Materials Science Research Institute, Chulalongkorn University ​

บรรณานุกรม

EndNote

APA

Chicago

MLA

ดิจิตอลไฟล์

Digital File
DOI Smart-Search
สวัสดีค่ะ ยินดีให้บริการสอบถาม และสืบค้นข้อมูลตัวระบุวัตถุดิจิทัล (ดีโอไอ) สำนักการวิจัยแห่งชาติ (วช.) ค่ะ